Characteristics | Testing method | Unit | Result |
---|---|---|---|
Length | EN 1848-1 | m | 10,0 |
Width | EN 1848-1 | m | 1,00 |
Straightness | EN 1848-1 | mm/10m | < 20 |
Mass per unit area | EN 1849-1 | kg/m2 | 4,5 |
Thickness | EN 1849-1 | mm | 3,5 |
Watertightness | EN 1928 | kPa | 60 |
Reaction to fire test | EN 13501-1 | Klasse | E |
Shear resistance of joints | EN 12317-1 | N/50mm | NPD |
Tensile force long./trans. | EN 12311-1 | N/50mm | 450/400 (±100/±100) |
Elongation at single-end breaking force | EN 12311-1 | % | 4/4 (±2/±2) |
Resistance to impact | EN 12691 | mm | NPD |
Resistance to static loading | EN 12730 | kg | NPD |
Resistance to tearing (nail shank) long./trans. | EN 12310-1 | N | NPD |
Flexibility at low temperatures | EN 1109 | °C | -10 |
Flow resistance at elevated temperature | EN 1110 | °C | 80 |
Watertightness transmission after artifical aging | EN 1928 | kPa | 60 |
Water vapour transmission | EN 1931 | Sd | > 1500 m |
Water vapour transmission after artifical aging | EN 1931 | Sd | > 1500 m |
NPD = No performance determined